Aluminium foil tape uses 0.05-0.1mm foil with pressure-sensitive adhesive in 40-120mm widths. Rubber adhesive up to 80C, acrylic up to about 120C. For insulation seams, air ducts and flue pipes.
Key Specifications
| Item | Parameter |
|---|---|
| 铝箔Thickness | 0.05 / 0.06 / 0.07 / 0.08 / 0.1mm |
| 总Thickness | 0.08~0.2mm(含胶层) |
| 常见Width | 40 / 50 / 60 / 75 / 100 / 120mm(可Custom) |
| Length | 20m / 30m / 45m / 50m 每卷 |
| 胶层类型 | 橡胶型(≤80℃)、丙烯酸型(约 120℃) |
| 剥离强度 | ≥10 N/25mm(按产品等级) |
Applications
- Insulation seam sealing
- HVAC duct and flue joints
- Water heaters and range hoods
- Refrigerator and freezer lines
- Underfloor heating film joints
For quotations, samples or custom cutting of Aluminum Foil Tape, contact Maosheng Sealing Materials (Hejian, China): WhatsApp +86 185 0317 3007, email 2072321766@qq.com. See the Aluminum Foil Tape product page for details.