Anti-static rubber sheet controls surface resistivity (10^6-10^9 ohm for dissipative, 10^3-10^5 ohm for conductive grades) per HG/T 2793-2023. 2-5mm thick, must be grounded via snaps and ground cords.
Key Specifications
| Item | Parameter |
|---|---|
| 表面电阻 | 抗静电型 10⁶~10⁹Ω;导电型 10³~10⁵Ω |
| 常用Thickness | 2 / 3 / 5mm(台垫多为 2~3mm,地垫 3~5mm) |
| 常见Specification | 台垫 1.0m / 1.2m 宽,10m 卷;地垫 1.0m / 1.2m 宽 |
| Material | NBR / SBR / PVC / Silicone(耐高温型) |
| Colour | 黑色、绿色、灰色、蓝色(表面层可浅色) |
| 配套 | 接地扣、接地线、铜箔条、接地端子 |
Applications
- Electronics assembly benches
- Server and equipment rooms
- Flammable and explosive areas
- Laboratories and clean rooms
- Precision instrument zones
For quotations, samples or custom cutting of Anti-static Rubber Sheet, contact Maosheng Sealing Materials (Hejian, China): WhatsApp +86 185 0317 3007, email 2072321766@qq.com. See the Anti-static Rubber Sheet product page for details.