Conveyor belts per GB/T 7984-2013: EP100 to EP630 N/mm strength series, 2-6 plies, widths 400-2500mm, top cover 2-12mm and bottom 1-5mm. Cover grades H/D/L for different abrasion levels.
Key Specifications
| Item | Parameter |
|---|---|
| 强度Series(N/mm) | EP100/125/150/160/200/250/300/350/400/450/500/550/630 |
| 帆布层数 | 2 / 3 / 4 / 5 / 6 层(NN 可达 10 层) |
| 带宽 | 400 / 500 / 650 / 800 / 1000 / 1200 / 1400 / 1600 / 1800 / 2000 / 2500mm |
| 上覆盖胶Thickness | 2.0~12mm(常用 3 / 4.5 / 6mm) |
| 下覆盖胶Thickness | 1.0~5mm(常用 1.5 / 2 / 3mm) |
| 覆盖胶等级 | H(拉伸≥24MPa)/ D(≥18MPa)/ L(≥15MPa) |
| 特殊型 | 耐热、耐油、阻燃、耐寒、耐酸碱、防滑人字纹 |
Applications
- Coal and metal mining
- Port bulk handling
- Cement and aggregate plants
- Power plant coal handling
- Chemical, grain and metallurgy lines