Conveyor Belt Specifications and Common Models Guide

Conveyor Belt Specifications and Common Models Guide

Conveyor belts per GB/T 7984-2013: EP100 to EP630 N/mm strength series, 2-6 plies, widths 400-2500mm, top cover 2-12mm and bottom 1-5mm. Cover grades H/D/L for different abrasion levels.

Key Specifications

Item Parameter
强度Series(N/mm) EP100/125/150/160/200/250/300/350/400/450/500/550/630
帆布层数 2 / 3 / 4 / 5 / 6 层(NN 可达 10 层)
带宽 400 / 500 / 650 / 800 / 1000 / 1200 / 1400 / 1600 / 1800 / 2000 / 2500mm
上覆盖胶Thickness 2.0~12mm(常用 3 / 4.5 / 6mm)
下覆盖胶Thickness 1.0~5mm(常用 1.5 / 2 / 3mm)
覆盖胶等级 H(拉伸≥24MPa)/ D(≥18MPa)/ L(≥15MPa)
特殊型 耐热、耐油、阻燃、耐寒、耐酸碱、防滑人字纹

Applications

  • Coal and metal mining
  • Port bulk handling
  • Cement and aggregate plants
  • Power plant coal handling
  • Chemical, grain and metallurgy lines

For quotations, samples or custom cutting of Conveyor Belt, contact Maosheng Sealing Materials (Hejian, China): WhatsApp +86 185 0317 3007, email 2072321766@qq.com. See the Conveyor Belt product page for details.

WhatsApp