Custom gaskets are produced to drawing or sample for non-standard equipment and special media. Flange types follow HG/T 20606 and spiral wound types HG/T 20610. Die cutting, waterjet and CNC routing available, tolerance +/-0.5mm.
Key Specifications
| Item | Parameter |
|---|---|
| 加工方式 | 刀模冲裁、剪板、水切割、数控雕刻、车削 |
| 尺寸Tolerance | 常规 ±0.5mm,精密件可达 ±0.2mm |
| Thickness Range | 0.5~50mm(按Material与设备能力) |
| 可选Material | NBR / EPDM / NR / CR / Silicone / 氟胶 / PTFE / 石墨 / 金属 |
| 起订量 | 刀模件按模费计,水切割与雕刻可单件起订 |
| 打样周期 | 常规 1~3 天出样,批量按数量排产 |
Applications
- Non-standard equipment sealing
- Import equipment localisation
- Reactor and heat exchanger flanges
- Pump, valve and instrument joints
- Reverse-engineered replacement parts
For quotations, samples or custom cutting of Custom Gaskets, contact Maosheng Sealing Materials (Hejian, China): WhatsApp +86 185 0317 3007, email 2072321766@qq.com. See the Custom Gaskets product page for details.