EPDM rubber sheet excels in weathering, ozone, steam and mild acid/alkali resistance. Service -40C to +120C, thickness 1-20mm. Not suitable for mineral oil – use NBR instead.
Key Specifications
| Item | Parameter |
|---|---|
| Thickness Range | 1 / 1.5 / 2 / 3 / 4 / 5 / 6 / 8 / 10 / 12 / 15 / 20mm |
| 常见Width | 1000 / 1200 / 1500mm |
| Service Temperature | -40℃ ~ +120℃(短时可达 150℃) |
| 硬度(邵氏A) | 50~80 度,常用 60 / 65 / 70 度 |
| 拉伸强度 | ≥7MPa(通用型) |
| 耐臭氧 | 远优于 NR/SBR,户外长期不龟裂 |
| Colour | 黑色为主,可Custom灰、白、红 |
Applications
- Roof and curtain wall sealing
- Outdoor cabinets and solar equipment
- Steam and hot water flanges
- Sewage and environmental plants
- Automotive and rail seals
For quotations, samples or custom cutting of EPDM Rubber Sheet, contact Maosheng Sealing Materials (Hejian, China): WhatsApp +86 185 0317 3007, email 2072321766@qq.com. See the EPDM Rubber Sheet product page for details.