Fabric Reinforced Rubber Sheet Technical Details
Fabric reinforced rubber sheet embeds 1-8 plies of canvas or nylon between rubber layers, greatly improving tear, extrusion and dimensional resistance. 2-30mm thick, for large low-pressure flanges and vibratory equipment.
| Item | Parameter |
|---|---|
| Thickness range | 2 / 3 / 4 / 5 / 6 / 8 / 10 / 12 / 15 / 20 / 25 / 30mm |
| Fabric plies | 1~8 层(常用 2~4 层) |
| Fabric type | 棉帆布、Nylon布、聚酯布、金属网 |
| Common width | 1000 / 1200 / 1500mm |
| Material | NR / SBR / NBR / EPDM(按介质选) |
Read the full technical guide: Fabric Reinforced Rubber Sheet specifications and common models.