Fireproof Mud (Flexible Organic Sealing Putty) Specifications and Common Models Guide

Fireproof Mud (Flexible Organic Sealing Putty) Specifications and Common Models Guide

Flexible organic fire sealing putty (DRK) per GB 23864-2023: grades A1/A2/A3 with A3 >=3h fire integrity and insulation, burning behaviour not below B2, density <=2.0x10^3 kg/m3, water and oil resistant for 3 days.

Key Specifications

Item Parameter
耐火等级 A1(≥1h)/ A2(≥2h)/ A3(≥3h,耐火完整性与隔热性均≥3.00h)
燃烧性能 不低于 GB 8624 规定的 B2 级
表观Density ≤2.0×10³ kg/m³
耐水性 / 耐油性 均≥3 天,不溶胀、不开裂
耐湿热性 ≥120h 不开裂、不粉化
耐冻融循环 ≥15 次不开裂、不粉化
常见包装 2kg / 块(塑料袋包装),整箱约 20kg

Applications

  • Cable wall and floor penetrations
  • Switchgear and control cabinet entries
  • Cable trenches and shafts
  • Substation cable interlayers
  • Petrochemical, tunnel and marine gaps