2026-09-24
Post

Asbestos / Fireproof Materials Specifications and Common Models Guide

Asbestos / Fireproof Materials Specifications and Common Models Guide

Asbestos rubber sheet follows GB/T 3985-2008 with grades XB450 (450C/6MPa), XB350 (350C/4MPa) and XB200 (200C/1.5MPa). Fireproof sealing putty follows GB 23864-2023 with class B2 burning behaviour.

Key Specifications

Item Parameter
石棉板Thickness 0.5 / 1 / 1.5 / 2 / 2.5 / 3 / 4 / 5 / 6mm
常见板幅 500×500、1000×1000、1500×2000mm(宽500/620/1200/1260/1500mm)
Service Temperature XB200≤200℃、XB350≤350℃、XB450≤450℃
使用压力 XB200≤1.5MPa、XB350≤4MPa、XB450≤6MPa
Fireproof Putty 表观Density≤2.0×10³ kg/m³,耐水/耐油≥3天,耐冻融≥15次
防火等级 Fireproof Putty燃烧性能不低于 B2 级,耐火可达 3h(A3 级)

Applications

  • Boiler and steam pipe flanges
  • Kiln and oven door seals
  • High-temperature pipe insulation wrapping
  • Cable penetration fire sealing
  • Substation and switchboard fire stops

For quotations, samples or custom cutting of Asbestos / Fireproof Materials, contact Maosheng Sealing Materials (Hejian, China): WhatsApp +86 185 0317 3007, email 2072321766@qq.com. See the Asbestos / Fireproof Materials product page for details.