Flame-retardant rubber sheet is self-extinguishing: FV-0/FV-1/FV-2 per GB/T 2408 vertical burning test, oxygen index >=28%. Thickness 1-10mm, for mining, power, marine and metro use.

Key Specifications

Item Parameter
常用Thickness 1 / 2 / 3 / 4 / 5 / 6 / 8 / 10mm
常见Width 1000 / 1200 / 1500mm
Flame Retardant Rating FV-0 / FV-1 / FV-2(按 GB/T 2408 垂直法)
氧指数 ≥28%(优质氯丁胶板可达 30% 以上)
Material CR 氯丁胶、EPDM、NBR 阻燃配方
Colour 黑色为主,可Custom警示色