Insulation Mat Specifications and Common Models Guide

Insulation Mat Specifications and Common Models Guide

Insulation mats protect personnel in switch rooms and substations. Per HG/T 2949-2023, thickness maps to voltage: 3mm/5kV, 5mm/10kV, 6mm/15kV, 8mm/20-25kV, 10mm/30kV, 12mm/35kV.

Key Specifications

Item Parameter
Thickness与电压 3mm/5kV、5mm/10kV、6mm/15kV、8mm/20~25kV、10mm/30kV、12mm/35kV
常规Width 1000 / 1200 / 1500mm
Length 5m / 10m 每卷,也可按米裁售
Colour 黑色、红色、绿色、黑绿复合(红平、绿平为配电室常见配色)
表面 平面、防滑细纹、圆扣纹(防滑型)
耐电压 按 HG/T 2949-2023 对应等级工频耐压试验