Spiral Wound Gasket Technical Details
Spiral wound gaskets combine metal winding with graphite or PTFE filler for medium/high pressure flanges. Per HG/T 20610-2009: types A/B/C/D, DN10-DN2000, PN1.6-PN100, 3.2/4.5mm thick, graphite filler to 550C.
| Item | Parameter |
|---|---|
| Nominal size DN | DN10 ~ DN2000 |
| Nominal pressure | PN1.6 / PN2.5 / PN6 / PN10 / PN16 / PN25 / PN40 / PN63 / PN100 |
| Gasket thickness | 3.2mm(常用)、4.5mm,另有 2.5 / 6.4 / 7.2mm |
| Metal strip material | 304、304L、316、316L、321、碳钢、钛、蒙乃尔等 |
| Filler material | 柔性石墨、聚PTFE乙烯(PTFE)、无石棉纸 |
Read the full technical guide: Spiral Wound Gasket specifications and common models.