Nylon Rod and Sheet Specifications and Common Models Guide

Nylon Rod and Sheet Specifications and Common Models Guide

Nylon rod and sheet (PA6 milky white, PA66, cast MC ivory) offer low friction and high wear resistance to replace bronze bushes. Rods 10-200mm, sheets 5-100mm, service -40C to +100C.

Key Specifications

Item Parameter
棒材直径 10 / 15 / 20 / 25 / 30 / 40 / 50 / 60 / 80 / 100 / 120 / 150 / 200mm 等
板材Thickness 5 / 8 / 10 / 12 / 15 / 20 / 25 / 30 / 40 / 50 / 60 / 80 / 100mm
板幅 500×500、600×1200、1000×2000mm(按牌号)
Density 1.14~1.16 g/cm³
Service Temperature -40℃ ~ +100℃(短时 120℃,玻纤增强可达 150℃)
Colour PA6 乳白色、MC 铸型象牙白(发黄为氧化次品色)
吸水率 PA6 吸水率较高,精密件需考虑尺寸变化

Applications

  • Bushes, bearings and slide blocks
  • Gears, sprockets and rollers
  • Conveyor wear liners
  • Crane and metallurgical pulleys
  • Food and packaging machine parts