Braided packing seals valve stems, pump shafts and agitators. Square sections from 3x3mm to 50x50mm (6×6 to 25×25 common), aramid/PTFE/graphite/carbon/hemp materials, -200C to +600C, up to 35MPa.
Key Specifications
| Item | Parameter |
|---|---|
| 截面Specification | 3×3、4×4、5×5、6×6、8×8、10×10、12×12、14×14、16×16、20×20、25×25mm 等 |
| 常用Specification | 6×6、8×8、10×10、12×12、16×16、20×20mm |
| Suitable温度 | -200℃ ~ +600℃(按Material,石墨类最高约 450~600℃) |
| Suitable压力 | 旋转泵约 3~25MPa,往复泵约 10MPa,阀门约 20~35MPa(按Material) |
| 线速度 | 0~15 m/s(按Material) |
| pH 范围 | 2~13(碳纤维可达 1~14) |
Applications
- Centrifugal and reciprocating pump shafts
- Gate, globe and ball valve stems
- Reactor and mixer shaft seals
- Marine stern tube sealing
- Steam and hot oil line valves
For quotations, samples or custom cutting of Packing, contact Maosheng Sealing Materials (Hejian, China): WhatsApp +86 185 0317 3007, email 2072321766@qq.com. See the Packing product page for details.