PVC crystal sheet is a rigid, high-gloss transparent PVC panel used for machine guards, windows, partitions and bench tops. Thickness 1-30mm, standard sheet 1220x2440mm, service -10C to +60C.
Key Specifications
| Item | Parameter |
|---|---|
| Thickness Range | 1 / 1.5 / 2 / 3 / 4 / 5 / 6 / 8 / 10 / 12 / 15 / 20 / 25 / 30mm |
| 常见板幅 | 1220×2440mm(可Custom 1000×2000 等) |
| Density | 1.35~1.45 g/cm³ |
| Service Temperature | -10℃ ~ +60℃(短时不超过 70℃) |
| 透光率 | 高光水晶板可达 85% 以上 |
| Colour | 透明、磨砂透明、蓝、绿、白、红 |
Applications
- Machine guards and sight windows
- Workshop partitions
- Lab and bench top liners
- Light boxes and display panels
- Plating and pickling tank linings