PVC Crystal Sheet Specifications and Common Models Guide

PVC Crystal Sheet Specifications and Common Models Guide

PVC crystal sheet is a rigid, high-gloss transparent PVC panel used for machine guards, windows, partitions and bench tops. Thickness 1-30mm, standard sheet 1220x2440mm, service -10C to +60C.

Key Specifications

Item Parameter
Thickness Range 1 / 1.5 / 2 / 3 / 4 / 5 / 6 / 8 / 10 / 12 / 15 / 20 / 25 / 30mm
常见板幅 1220×2440mm(可Custom 1000×2000 等)
Density 1.35~1.45 g/cm³
Service Temperature -10℃ ~ +60℃(短时不超过 70℃)
透光率 高光水晶板可达 85% 以上
Colour 透明、磨砂透明、蓝、绿、白、红

Applications

  • Machine guards and sight windows
  • Workshop partitions
  • Lab and bench top liners
  • Light boxes and display panels
  • Plating and pickling tank linings