Flexible elastomeric thermal insulation per GB/T 17794-2008: class I (oxygen index >=32%) and class II (>=26%), thermal conductivity <=0.036 W/(mK) at 0C, service -40C to +110C. Sheets 10-50mm, tubes 6-108mm ID x 2m.

Key Specifications

Item Parameter
板材Thickness 10 / 15 / 20 / 25 / 30 / 40 / 50mm(常规 6~50mm)
板材Width 1000 / 1200 / 1500mm
管材Inner Diameter 6 / 10 / 13 / 16 / 20 / 22 / 25 / 28 / 34 / 43 / 48 / 60 / 76 / 89 / 108mm
管材壁厚 10 / 15 / 20 / 25 / 30mm,Length 2m/根
导热系数 0℃时 ≤0.036 W/(m·K)(-20℃≤0.034、40℃≤0.041)
Service Temperature -40℃ ~ +110℃
燃烧性能 Ⅰ类氧指数≥32%;建筑用不低于 GB 8624-2006 C 级(B1 难燃)

Applications

  • Chilled and condensate water pipes
  • Hot water and heating pipes
  • Air ducts and AHU casings
  • Cold storage and refrigerated trucks
  • Solar and heat pump pipework