Flexible elastomeric thermal insulation per GB/T 17794-2008: class I (oxygen index >=32%) and class II (>=26%), thermal conductivity <=0.036 W/(mK) at 0C, service -40C to +110C. Sheets 10-50mm, tubes 6-108mm ID x 2m.
Key Specifications
| Item | Parameter |
|---|---|
| 板材Thickness | 10 / 15 / 20 / 25 / 30 / 40 / 50mm(常规 6~50mm) |
| 板材Width | 1000 / 1200 / 1500mm |
| 管材Inner Diameter | 6 / 10 / 13 / 16 / 20 / 22 / 25 / 28 / 34 / 43 / 48 / 60 / 76 / 89 / 108mm |
| 管材壁厚 | 10 / 15 / 20 / 25 / 30mm,Length 2m/根 |
| 导热系数 | 0℃时 ≤0.036 W/(m·K)(-20℃≤0.034、40℃≤0.041) |
| Service Temperature | -40℃ ~ +110℃ |
| 燃烧性能 | Ⅰ类氧指数≥32%;建筑用不低于 GB 8624-2006 C 级(B1 难燃) |
Applications
- Chilled and condensate water pipes
- Hot water and heating pipes
- Air ducts and AHU casings
- Cold storage and refrigerated trucks
- Solar and heat pump pipework
For quotations, samples or custom cutting of Rubber Plastic Insulation, contact Maosheng Sealing Materials (Hejian, China): WhatsApp +86 185 0317 3007, email 2072321766@qq.com. See the Rubber Plastic Insulation product page for details.