Sealing strips for doors, windows and curtain walls follow GB/T 24498-2009. EPDM grades marked EPDM60-4-3 (hardness-recovery-aged recovery); tensile >=5.0MPa (>=10.3MPa for curtain wall), compression set <=35%, no crack at -40C.
Key Specifications
| Item | Parameter |
|---|---|
| 常用断面 | D 型、E 型、P 型、O 型、9×9、7×8 等(可开模Custom) |
| Material | EPDM 三元乙丙、VMQ Silicone、PVC/PPVC、TPE |
| 硬度(邵氏A) | 55~75 度,常用 60±5 度 |
| 拉伸强度 | ≥5.0MPa(幕墙用胶条 ≥10.3MPa) |
| Service Temperature | EPDM -50~+120℃;Silicone -60~+200℃ |
| 压缩永久变形 | 100℃×168h、25%压缩率条件下 ≤35% |
| 低温脆性 | -40℃ 不破裂 |
Applications
- Windows, doors and curtain walls
- Automotive doors and hatches
- Electrical cabinets and enclosures
- Machine covers and access doors
- Cold room and clean room doors
For quotations, samples or custom cutting of Rubber Sealing Strip, contact Maosheng Sealing Materials (Hejian, China): WhatsApp +86 185 0317 3007, email 2072321766@qq.com. See the Rubber Sealing Strip product page for details.