Hejian Maosheng Sealing Materials Co., Ltd. is a direct manufacturer of anti-slip rubber sheet in Hejian City, Hebei, China, producing wide rib, fine rib, studded, diamond, cloth pattern and smooth finish sheets. Our anti-slip rubber sheets use NR, SBR and CR rubber as the base material, offering good elasticity, wear and pressure resistance and stable anti-slip performance, supplied on a long-term basis for workshop floors, truck bed linings, stair treads, machine guards, elevator mats and gyms. As a Hebei anti-slip rubber sheet factory we cut any size from 2-20 mm thick and 1000-2000 mm wide, and also supply flat sheets and custom die-cut parts.
Specifications
| Item | Parameter Range | Description |
|---|---|---|
| Material | NR / SBR / CR (selected on request) | Oil, cold and anti-static grades available |
| Thickness | 2 – 20 mm | Non-standard customization available |
| Standard Width | 1000 / 1200 / 1500 / 2000 mm | Cut to any width |
| Surface Pattern | Wide Rib / Fine Rib / Studded / Diamond / Cloth / Smooth | Recommended by scenario |
| Shore Hardness | 60 – 75 A | Adjustable on request |
| Service Temperature | -20 ℃ ~ +80 ℃ | Varies by material |
| Colour | Black / Red / Green / Yellow (to colour chart) | RAL colour chart available |
| Standard | GB/T 5574 etc. | Produced to customer requirement |
Application Cases
- Workshop Flooring / Workbench Laying Anti-slip, anti-fatigue, sound absorbing.
- Vehicle / Cargo Bed Linings Anti-slip and wear resistant, protecting goods and personnel.
- Stair Treads / Platforms Anti-slip safety, reducing fall risk.
- Equipment Guards / Machine Surrounds Damping, anti-slip, easy to clean.
- Gyms / Warehouse Mats Impact resistant, protects floors.
Our Advantages
- Hejian direct factory, any thickness from 2 to 20 mm with all surface patterns in stock, recommending the best option for your scenario.
- Cut to length, custom die-cutting and adhesive backing, ready to install.
- Stock sizes shipped the same day, bulk orders scheduled by lead time.
- Complete wear and pressure test reports with material certification.
- 13% VAT invoices available, monthly settlement for long-term partners.
Need an anti-slip rubber sheet specification sheet or a sample? Contact us for a quotation.