FKM Fluororubber Sheet

氟橡胶板耐高温、耐强酸碱和多种溶剂,适合化工、制药和高温工况的密封与衬垫。

FKM fluororubber sheet for high temperature and aggressive chemical sealing.

Overview

产品摘要

Product Overview

氟橡胶板以 FKM 氟橡胶为原料,耐高温、耐强酸碱和多种有机溶剂,在苛刻介质工况下仍能保持弹性,常用于化工设备密封、制药管线垫片和高温衬垫。

FKM fluororubber sheet resistant to high temperature, acids, alkalis and solvents for chemical sealing.

说明 氟橡胶板以 FKM 氟橡胶为原料,耐高温、耐强酸碱和多种有机溶剂,在苛刻介质工况下仍能保持弹性,常用于化工设备密封、制药管线垫片和高温衬垫。 FKM fluororubber sheet resistant to high temperature, acids, alkalis and solvents for chemical sealing.
常用类型 氟橡胶板、FKM 氟胶板 FKM and fluoro rubber sheet
适用工况 高温、强酸碱、有机溶剂 High temperature, acids and solvents
规格范围 厚度 1~30mm,宽度/长度可定制 1-30mm thick, custom width and length
可定制项 厚度、尺寸、硬度与颜色 Thickness, size, hardness and colour
Tech Guide

技术详解:执行标准与常用型号

Technical Guide: Standards & Common Models

按现行国家标准整理的执行标准、常用型号与选型要点,供采购与技术人员选型参考。

Current GB/HG standards, common models and selection tips for buyers and engineers.

氟橡胶板技术详解:GB/T 5574-2008(特种)+ HG/T 2811 体系

氟橡胶板(FKM)属 GB/T 5574-2008 特种胶板,使用温度 -20~+250℃(短时 300℃),拉伸强度 8~15MPa、硬度 75±5 邵A、压缩永久变形<30%,耐强酸强碱与油类,厚度 0.5~25mm。

型号/牌号说明
通用型 FKM 板黑色,硬度 75 邵A,-20~+250℃,化工设备通用密封
耐高温型 FKM长期 250℃、短时 300℃,发动机与高温管路
食品级 FKM 板蓝/灰白色,符合食品接触迁移要求,医药食品设备
夹布 FKM 板夹布增强,抗挤出,高压法兰与反应釜