产品详情
Product Details

B1B2级橡塑管

B1/B2 Rubber-plastic Insulation Tube

B1/B2 级难燃橡塑保温管,闭孔发泡结构,导热系数低、柔软易安装,用于空调冷冻水、冷凝水与热水管道保温,管内径 6~108mm 常备。

B1/B2 fire-rated NBR/PVC elastomeric insulation tubes with closed-cell foam, for chilled water and HVAC piping, 6-108mm bore in stock.

Overview

产品摘要

Product Overview

橡塑保温管以 NBR/PVC 为基材闭孔发泡成型,B1 级难燃(氧指数≥32%)、B2 级可选,导热系数 0℃ 时 ≤0.036 W/(m·K),使用温度 -40~+110℃。常备管内径 6~108mm、壁厚 10~30mm、长度 2m/根,套管式安装、可裁切,广泛用于中央空调冷冻水、冷凝水与热水管道保温。

B1/B2 fire-rated NBR/PVC elastomeric insulation tubes (oxygen index >=32% for B1), closed-cell foam, 6-108mm bore, 10-30mm wall, 2m lengths, for chilled water, condensate and hot water piping.

说明 橡塑保温管以 NBR/PVC 为基材闭孔发泡成型,B1 级难燃(氧指数≥32%)、B2 级可选,导热系数 0℃ 时 ≤0.036 W/(m·K),使用温度 -40~+110℃。常备管内径 6~108mm、壁厚 10~30mm、长度 2m/根,套管式安装、可裁切,广泛用于中央空调冷冻水、冷凝水与热水管道保温。 B1/B2 fire-rated NBR/PVC elastomeric insulation tubes (oxygen index >=32% for B1), closed-cell foam, 6-108mm bore, 10-30mm wall, 2m lengths, for chilled water, condensate and hot water piping.
常用类型 B1 级难燃橡塑管、B2 级橡塑管、带铝箔贴面 B1/B2 tubes and foil-faced type
适用工况 空调冷冻水、冷凝水、热水管道与风管保温 Chilled water, condensate and HVAC piping
规格范围 内径 6~108mm,壁厚 10~30mm,2m/根 6-108mm bore, 10-30mm wall, 2m lengths
执行标准 GB/T 17794-2008 柔性泡沫橡塑绝热制品 GB/T 17794-2008
可定制项 内径、壁厚、贴面与长度 Bore, wall, facing and length
Tech Guide

技术详解:执行标准与常用型号

Technical Guide: Standards & Common Models

按现行国家标准整理的执行标准、常用型号与选型要点,供采购与技术人员选型参考。

Current GB/HG standards, common models and selection tips for buyers and engineers.

B1B2级橡塑管技术详解:GB/T 17794-2008

B1B2级橡塑管执行 GB/T 17794-2008,B1 级难燃(氧指数≥32%)、B2 级可选,管内径 6~108mm、壁厚 10~30mm、2m/根,导热系数 0℃ 时 ≤0.036 W/(m·K),使用温度 -40~+110℃。

型号/牌号说明
B1 级难燃管(Ⅰ 类)氧指数≥32%、烟密度≤75,建筑与人员密集场所消防验收常用
B2 级橡塑管(Ⅱ 类)氧指数≥26%,一般工业管道保温
带铝箔贴面管复合铝箔,抗老化隔汽,室外与明装管道
壁厚 15 / 20 / 25 / 30mm常用壁厚档,按防结露与保温要求选

完整执行标准、规格表与选型建议,请阅读技术文章《B1B2级橡塑管规格型号指南》。