Asbestos rubber sheet per GB/T 3985-2008: XB450 (450C/6MPa), XB350 (350C/4MPa), XB200 (200C/1.5MPa). Oil grades per GB/T 539-2008: NY400/NY250/NY150. Thickness 0.5-6mm, width 500-1500mm.
Key Specifications
| Item | Parameter |
|---|---|
| Thickness Range | 0.5 / 0.8 / 1 / 1.5 / 2 / 2.5 / 3 / 4 / 5 / 6mm |
| 常见Width | 500 / 620 / 1200 / 1260 / 1500mm |
| Service Temperature | XB200≤200℃、XB350≤350℃、XB450≤450℃;NY150/250/400 对应 150/250/400℃ |
| 使用压力 | XB200≤1.5MPa、XB350≤4MPa、XB450≤6MPa |
| 耐油型压力 | NY150≤1.5MPa、NY250≤2.5MPa、NY400≤4MPa |
| Colour标识 | XB450 紫、XB350 红、XB200 灰;NY400 石墨色、NY250 浅蓝、NY150 灰白 |
Applications
- Boiler and steam pipe flanges
- Heat transfer oil systems
- Petrochemical low/medium pressure flanges
- Oil and solvent tank connections
- Marine and power plant flanges
For quotations, samples or custom cutting of Asbestos Rubber Sheet, contact Maosheng Sealing Materials (Hejian, China): WhatsApp +86 185 0317 3007, email 2072321766@qq.com. See the Asbestos Rubber Sheet product page for details.