Oil-resistant rubber sheet (NBR) resists swelling in mineral oil, transformer oil and petrol. Grades 3707/3807 (7MPa) and 3709/3809 (9MPa) per GB/T 5574-2008, thickness 0.5-20mm, service -30C to +100C.
Key Specifications
| Item | Parameter |
|---|---|
| Thickness Range | 0.5 / 1 / 1.5 / 2 / 2.5 / 3 / 4 / 5 / 6 / 8 / 10 / 12 / 14 / 16 / 18 / 20mm |
| Width | 500~2000mm(常用 1000 / 1200 / 1500mm) |
| Service Temperature | -30℃ ~ +100℃ |
| 拉伸强度 | 7MPa(3707/3807)或 9MPa(3709/3809) |
| 硬度(邵氏A) | 60~80 度(按牌号第二位区分档) |
| Suitable Media | 机油、变压器油、汽油、润滑油、液压油 |
| Colour | 黑色为主,另有黄、红、蓝、绿(老标区分色) |
Applications
- Gearbox and oil tank flanges
- Transformer and oil-filled equipment
- Hydraulic and lubrication systems
- Fuel stations and tank farms
- Automotive oil pans and seals
For quotations, samples or custom cutting of Oil-resistant Rubber Sheet, contact Maosheng Sealing Materials (Hejian, China): WhatsApp +86 185 0317 3007, email 2072321766@qq.com. See the Oil-resistant Rubber Sheet product page for details.