Product Details
Product Details

B1/B2 Rubber-plastic Insulation Tube

B1/B2 Rubber-plastic Insulation Tube

B1/B2 fire-rated NBR/PVC elastomeric insulation tubes with closed-cell foam, for chilled water and HVAC piping, 6-108mm bore in stock.

B1/B2 fire-rated NBR/PVC elastomeric insulation tubes with closed-cell foam, for chilled water and HVAC piping, 6-108mm bore in stock.

Overview

Product Summary

Product Overview

B1/B2 fire-rated NBR/PVC elastomeric insulation tubes (oxygen index >=32% for B1), closed-cell foam, 6-108mm bore, 10-30mm wall, 2m lengths, for chilled water, condensate and hot water piping.

B1/B2 fire-rated NBR/PVC elastomeric insulation tubes (oxygen index >=32% for B1), closed-cell foam, 6-108mm bore, 10-30mm wall, 2m lengths, for chilled water, condensate and hot water piping.

Description B1/B2 fire-rated NBR/PVC elastomeric insulation tubes (oxygen index >=32% for B1), closed-cell foam, 6-108mm bore, 10-30mm wall, 2m lengths, for chilled water, condensate and hot water piping. B1/B2 fire-rated NBR/PVC elastomeric insulation tubes (oxygen index >=32% for B1), closed-cell foam, 6-108mm bore, 10-30mm wall, 2m lengths, for chilled water, condensate and hot water piping.
Common Types B1/B2 tubes and foil-faced type B1/B2 tubes and foil-faced type
Operating Conditions Chilled water, condensate and HVAC piping Chilled water, condensate and HVAC piping
Size Range 6-108mm bore, 10-30mm wall, 2m lengths 6-108mm bore, 10-30mm wall, 2m lengths
Standard GB/T 17794-2008 GB/T 17794-2008
Customization Bore, wall, facing and length Bore, wall, facing and length
Tech Guide

技术详解:Standard与常用Model

Technical Guide: Standards & Common Models

按现行国家标准整理的Standard、常用Model与选型要点,供Purchasing与技术人员选型参考。

Current GB/HG standards, common models and selection tips for buyers and engineers.

B1/B2 Rubber-plastic Insulation Tube Technical Details

B1/B2 fire-rated elastomeric NBR/PVC insulation tubes per GB/T 17794-2008: 6-108mm bore, 10-30mm wall, 2m lengths, thermal conductivity <=0.036 W/(mK) at 0C, service -40C to +110C.

ItemParameter
管Inner Diameter6 / 10 / 13 / 16 / 20 / 22 / 25 / 28 / 34 / 43 / 48 / 60 / 76 / 89 / 108mm
壁厚10 / 15 / 20 / 25 / 30mm(常规 6~50mm 可定)
Length2m/根(整箱供货)
Thermal conductivity0℃ 时 ≤0.036 W/(m·K)(-20℃≤0.034、40℃≤0.041)
Service temperature-40℃ ~ +110℃

Read the full technical guide: B1/B2 Rubber-plastic Insulation Tube specifications and common models.